FeNi Soft Magnetic Alloy

FeNi Soft Magnetic Alloy
Product Detailed
Related Categories:Agricultural Product Stock
FeNi Soft Magnetic AlloyFeNi Soft Magnetic Alloy (GBn198-1988)Grade & Chemical Composition (see Table 1) Table 1 Grade & Chemical CompositionSortGradeChemical Composition (%)CPSMnSiNiCrCoMoCuFeHigh magnetic conductivity higher saturation magnetic flux density soft magnetic alloy1J460.030.0200.020.60~1.10.15~0.345.0~46.50.20Balance1J500.30~0.60.15~0.349.0~50.50.201J540.30~0.61.10~1.4049.0~51.03.80~4.20.20High initial permeability of soft magnetic alloy1J760.30~0.600.15~0.375.0~76.51.80~2.24.80~5.21J770.30~0.600.15~0.375.0~783.9~4.54.80~61J790.60~1.10.30~0.5078.5~80.03.80~4.100.201J800.60~1.11.10~1.579.0~81.02.6~3.00.201J850.030.0200.020.30~0.600.15~0.379.0~81.04.80~5.200.201J861.000.3080.5~81.55.80~6.2Moment magnetic alloy1J340.30~0.600.15~0.3033.5~35.028.5~302.80~3.20.201J510.30~0.600.15~0.3049.0~50.51J520.30~0.600.15~0.3049.0~50.51.80~2.21J650.30~0.600.15~0.3064.5~66.01J670.30~0.600.15~0.3064.5~66.01.80~2.21J830.30~0.600.15~0.3078.5~79.52.80~3.21J4030.30~0.600.15~0.3039.0~ 41.024.5~25.53.80~4.23.80~4.2Mechanical Property (see Table 2)Table 2 Mechanical PropertyGradeResisitivity      (  m )Desinty(g/cm3)Curie Point       CHigh Saturated magneto-striction coefficient       /10-6Brinell hardness      HBSb Tensile Strength      MPas Yield Strength      MPaElongation      (%)unan-nealedan-nealedunan-nealedan-nealedunan-nealedan-nealedunan-nealedan-nealed1J460.458.24002517013073573531J500.458.2500251701307854506851503371J540.98.2360-1901258855008351502401J4030.558.55600---------1J760.558.64002.4--------1J770.558.6350---980540--2401J790.558.6450221012010305609801503501J800.628.53300.52401309305608851504401J850.568.754000.5--------1J860.608.85----------1J340.58.7-----540---421J510.458.2500----450---371J52-8.2----------1J650.258.35600----540---431J670.458.48530---930540--3501J830.508.6460---1030490--350Physical Property (See Table 3 & Table 4) Table 3 Average Coefficient of Linear ExpansionGradeCoefficient of Linear Expansion at Different Temperature/( 10-6/K)20~      100 C20~      200 C20~      300 C20~      400 C20~      500 C20~      600 C20~      700 C20~      800 C20~      900 C1J508.99.279.29.29.41J7910.3~10.810.9~11.211.4~12.911.9~12.512.3~13.212.7~13.413.1~13.613.4~13.613.2~13.71J8012.8~13.012.5~12.713.1~13.413.4~13.813.9~14.414.2~14.814.5~15.215.0~15.615.5~15.6Note: 1. Saturated magnetic induction,Website:http://www.astrongmagnet.com, Bs, is measured under 2000~2400 A/m applied magnetism for 1J34, 1J51, 1J52 and 1J403. 800 A/m for 1J65, 1J67 and 1J83.2. Iron loss P1/400 and P1/300 represent iron loss when peak magnetic induction reaches 1T at 400 Hz and 300 Hz, respectively.3. Bm in Square coefficient Br/Bm represents magnetic induction strength under 80 A/m applied magnetic strength.


Copyright Notice @ 2008-2022 ECBAY Limited and/or its subsidiaries and licensors. All rights reserved.